# Through-hole joint inspection: ARGYNIX bench checklist

ARGYNIX Skills (worldskills.blog), lesson "Through-hole joints you would sign off".
Our own practice checklist, written by ARGYNIX. It is not IPC-A-610 and not an official
marking scheme. For the industry's acceptance limits, use your own copy of IPC-A-610.

Inspect at 5x to 10x, with light from two sides. Look at every joint in this order.
Mark each joint OK, or write the defect code and its cause in the joint log.

## The look order

1. **Wetting at the pad.** The solder meets the pad at a low angle and spreads to its edge.
   A ball sitting on the pad, or a dark ring where solder stops: reject (code NW).
2. **Wetting at the lead.** The solder climbs the lead in a smooth curve. A gap where
   solder pulls away from the lead: reject (code NW).
3. **Hole fill.** Look at the component side. On a plated hole you should see solder at
   the top of the barrel, around the lead. None: reject (code HF).
4. **Shape.** Concave fillet, lead outline visible. Convex blob that hides the lead:
   reject (code EX). Too little to make a fillet all round: reject (code IN).
5. **Surface.** Leaded solder: smooth and bright. SAC305: smooth, a little satin, which is
   normal. Grainy, cracked or rough: reject (code CD, a cold or disturbed joint).
6. **Holes and spikes.** A pinhole or blowhole in the fillet: reject (code BH). A point
   left where the iron came off: reject (code SP).
7. **Lead end.** Cut clean, protruding the length your task sets (our bench target is
   1.0 to 1.5 mm). Cut into the fillet, or too long: reject (code PR).
8. **Around the joint.** Solder balls, splashes, flux left on, bridges to the next pad:
   reject (code BR for a bridge, CL for residue or balls).
9. **The board.** Lifted pad, burnt or blistered board, melted mask or part body:
   reject (code DM). Stop and find out why before the next joint.
10. **The part.** Flat on the board, or at the height the drawing asks. Straight.
    Markings readable the same way. Polarity right: reject (code PL) if not.

## Defect codes

| Code | Defect | Usual cause | Fix |
|---|---|---|---|
| NW | Non-wetting or dewetting | Too little heat, dirty or oxidised pad or lead, no flux left | Flux, reheat pad and lead together, feed fresh solder |
| HF | Poor hole fill | Pad on a plane, tip too small, too short a time | Bigger tip, preheat the board, heat from the side with the plane |
| EX | Excess solder | Fed too much, too thick a wire | Wick off the excess, reflow with flux |
| IN | Insufficient solder | Fed too little | Add flux and a little solder |
| CD | Cold or disturbed joint | Lead moved while it cooled, or too little heat | Flux and reflow, hold still until it sets |
| BH | Blowhole or pinhole | Gas from the hole, often a damp board | Reflow with flux; dry damp boards before soldering |
| SP | Spike | Flux burnt off, iron pulled away slowly | Flux and reflow, lift the iron away cleanly |
| PR | Wrong protrusion | Cut too long, too short, or into the fillet | Re-cut; if cut into the fillet, reflow |
| BR | Bridge | Too much solder, tip dragged across | Flux and drag away, or wick |
| CL | Residue, balls, splashes | Flux not cleaned, wet sponge spitting | Clean with IPA and a brush, remove balls |
| DM | Damage | Too hot, too long, leverage on the lead | Stop. Repair as a separate job and record it |
| PL | Wrong polarity or part | Not checked before soldering | Remove and refit the right way |